• 1.0mm Afk502 Soft Magnetic Wire Permendur Alloy Wires
  • 1.0mm Afk502 Soft Magnetic Wire Permendur Alloy Wires
  • 1.0mm Afk502 Soft Magnetic Wire Permendur Alloy Wires
  • 1.0mm Afk502 Soft Magnetic Wire Permendur Alloy Wires
  • 1.0mm Afk502 Soft Magnetic Wire Permendur Alloy Wires
  • 1.0mm Afk502 Soft Magnetic Wire Permendur Alloy Wires

1.0mm Afk502 Soft Magnetic Wire Permendur Alloy Wires

Product Type: Wire
Material: Fecov
Carbon Content: Low Carbon
Surface: Bright
Condition: Soft / Hard
Diameter: 0.5mm-2.0mm
Samples:
US$ 35/Piece 1 Piece(Min.Order)
| Request Sample
Customization:
Diamond Member Since 2016

Suppliers with verified business licenses

Rating: 5.0/5
Manufacturer/Factory

Basic Info.

Model NO.
1J22
Package
Wooden Case
Shape
Wire
Main Chemical Composition
Co50V2
Density
8.2
Resistivity
0.4
Curie Point
980
Saturation Magnetostriction Coefficient
60~100
Applicant
Relay, Transducer
Transport Package
Coil, Waterproof Paper, Wooden Case
Specification
RoHs
Trademark
HUONA
Origin
Shanghai, China
HS Code
7505120000
Production Capacity
3000 Tons/Year

Product Description

1J22-Co50V2-Hiperco 50 - FeCoV Soft Magnetic Alloy Bar/Sheet/Strip 

Description :

Co50V2 Iron Cobalt is high saturation magnetic induction intensity of iron, cobalt, vanadium soft magnetic alloy in existing soft magnetic alloy calcium alloy has the highest saturated magnetic induction intensity (2.4 T), and high Curie temperature (980 ºC), saturation magnetostriction coefficient of maximum (60 ~ 100 * 10-6).

Due to the high saturation magnetic induction intensity, when making an equal power of motor, can greatly reduce the volume, when making electromagnet, under the same cross-sectional area can produce larger suction force.

Due to their high Curie point, can make the alloy can be in other soft magnetic alloy material has been completely demagnetization work under the high temperature, and maintain good magnetic stability.

Due to the large magnetostrictive coefficient, and is suitable for used as a magnetostrictive transducer, output energy is high, the efficiency is high.The resistivity of low alloy (0.27 mu Ω m.), is not suitable for use under high frequency.Price is more expensive, easily oxidized, processing performance is poor, adding suitable nickel or other elements, can improve the processing performance.

Application: suitable for making quality is light, small volume of aviation and space flight with electrical components, such as, micro-motor rotor magnet pole head, relays, transducers, etc

Chemical Content(%)
Mn Ni V C Si P S Fe Co
0.30 0.50 0.8-1.80 0.04 0.30 0.020 0.020 Bal 49.0-51.0

Mechanical Properties
Density 8.2 g/cm3
Thermal Expansion Coefficient (20~100ºC) 8.5 x 10-6 /ºC 
Curie Point  980ºC
Volume Resistivity (20ºC) 40 μΩ.cm
Saturation Magnetic Stricture Coefficient   60 x 10-6
Coercive Force  128A/m

Magnetic induction strength in different magnetic field
B400 1.6
B800 1.8
B1600 2.0
B2400 2.1
B4000 2.15
B8000 2.35

Packing Detail
 1). Coil (plastic spool) + compressed ply-wooden case + pallet 
 2). Coil (plastic spool) + carton + pallet  

Our Services
1.> We will reply within 24 hours after receiving the message.
2.> Professional sales team, English,Korean and Spanish talents provide outstanding service
3.> We accpet small quantity order to supports our Cooperation.
4.> We can offer OEM ODM service.
1.0mm Afk502 Soft Magnetic Wire Permendur Alloy Wires
1.0mm Afk502 Soft Magnetic Wire Permendur Alloy Wires
1.0mm Afk502 Soft Magnetic Wire Permendur Alloy Wires
 

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now