Material: | Wood Pulp |
---|---|
Usage: | Air Filter |
Thickness: | 0.61-0.9mm |
Basic Weight: | 101-150g/m² |
Corrugation Depth: | 0.45mm |
Resin Content: | 25.1%-30% |
Samples: |
---|
Customization: |
---|
Suppliers with verified business licenses
Parameters | ||||||
Application car model | Auto oil filtration | |||||
Product Model | LGOP-20848-YBL | |||||
Specifications | Test standard | |||||
Grammage | 208±10 g/m2 | GB/T451.2-2002 | ||||
Air Permeability | 480±60 L/m2•s | GB/T25453-1997 | ||||
Moisture | 3±2 % | / | ||||
Corrugation Depth | 0.40 ± 0.1 mm | GB/T451.3-2002 | ||||
Thickness | 0.9 ± 0.1 mm | GB/T24218.2-2009 | ||||
Burst Strength | SD - before curing > 220ºC | GB/T454-2002 | ||||
SDC - After curing > 230ºC | ||||||
Stiffness | SD - Before curing > 10 ºC | GB/T22364-2008 | ||||
SDC-After Curing > 14 ºC | ||||||
Pore size | Max pore size: 85 ± 10 μm | GB/T2679.14-1996 | ||||
Mean pore size: 80±10 μm | ||||||
Dust Hold Capacity | Flow rate: 4 L/min | / | ||||
Initial Pressure | Dust Added A3 Fine | ISO4548-12 | ||||
Characteristics | Phenol impregnated Filter Paper | |||||
Curing condition | 10min@170ºC |