Feature: | Oxidative Degradable |
---|---|
CAS No.: | 32131-17-2 |
Formula: | (C12h22n2o2)N |
Samples: |
---|
Customization: |
---|
Shipping Cost:
Estimated freight per unit. |
about shipping cost and estimated delivery time. |
---|
Payment Method: | |
---|---|
Initial Payment Full Payment |
Currency: | US$ |
---|
Return&refunds: | You can apply for a refund up to 30 days after receipt of the products. |
---|
Suppliers with verified business licenses
Polyamine Nylon 6 Thermal conductive material Flame Retardant Heat Stabilized
https://forever-plastics.en.made-in-china.com/product/rJwRvlcdZpWD/China-Nylon-PA6-GF33-PA66-Granules-PA6-with-30GF-Polyamide-PA66-30-GF-PA6-Material.html Heat-conducting nylon
Product Description | ||
Thermal conductive material, Flame Retardant, Heat Stabilized | ||
General | ||
Form Resin Pellets | ||
Feature Thermally Conductive Good Thermal | ||
UL Yellow Card E47960-101905729 | ||
Physical Nominal Value Test Method | ||
Density, dry 1.56 g/cm³ ISO 1183 | ||
Dry: Molding Shrinkage, Across Flow 0.45 % ISO 294-4 | ||
Dry: Molding Shrinkage, Flow 0.45 % ISO 294-4 | ||
Dry: Water Absorption, Saturation(23 °C) 6.0 % ISO 62 | ||
Dry: Water Absorption, Equilibrium(50% RH;23 °C) 1.6 % ISO 62 | ||
Mechanical Nominal Value Test Method | ||
Dry: Tensile Modulus 8000 MPa ISO 527-2 | ||
Condition: Tensile Modulus 3500 MPa ISO 527-2 | ||
Dry: Tensile Stress, Break 75.0 MPa ISO 527-2 | ||
Condition: Tensile Stress, Break 40.0 MPa ISO 527-2 | ||
Dry: Tensile Strain, Break 2.5 % ISO 527-2 | ||
Condition: Tensile Strain, Break 4.0 % ISO 527-2 | ||
Dry: Charpy Notched Impact Strength ISO 179 1eA | ||
-30 °C 2.0 kJ/m² | ||
23 °C 2.0 kJ/m² | ||
Condition: Charpy Notched Impact Strength ISO 179 1eA | ||
-30 °C 2.0 kJ/m² | ||
23 °C 2.0 kJ/m² | ||
Dry: Charpy Unnotched Impact Strength ISO 179 1eU | ||
-30 °C 40 kJ/m² | ||
23 °C 40 kJ/m² | ||
Condition: Charpy Unnotched Impact Strength ISO 179 1eU | ||
-30 °C 40 kJ/m² | ||
23 °C 60 kJ/m² | ||
Thermal | Nominal Value | Test Method |
Dry: Heat Deflection Temperature, Unannealed 0.45 MPa 1.8 MPa |
205 °C 140 °C |
ISO 75-2/B ISO 75-2/A |
Dry: Melting Temperature(10 °C/min) | 220 °C | ISO 11357-3 |
Dry: CLTE, Flow | 5.0E-5 cm/cm/°C | ISO 11359-2 |
Dry: CLTE, Transverse | 5.0E-5 cm/cm/°C | ISO 11359-2 |
Dry: Flammability Classification 1.2 mm 1.5 mm |
V-0 V-0 |
IEC 60695-11-10, - 20 |
Dry: Glow Wire Flammability Index(1.5 mm) | 960 °C | IEC 60695-2-12 |
Electrical | Nominal Value | Test Method |
Condition: Surface resistivity | 1.0E+13 ohms | IEC 60093 |
Dry: Volume Resistivity | 1.0e+14 ohms ·cm | IEC 60093 |
Condition: Volume resistivity | 1.0E+12 ohms ·cm | IEC 60093 |
Dry: Electric Strength | 30 kV/mm | IEC 60243-1 |
Condition: Electric Strength | 25 kV/mm | IEC 60243-1 |
Dry: Relative permittivity 100 Hz 1.0e+6 Hz |
3.60 3.20 |
IEC 60250 |
Condition: Relative Permittivity 100 Hz 1.0e+6 Hz |
10.0 3.70 |
IEC 60250 |
Dry: Dissipation Factor 100 Hz 1.0e+6 Hz |
8.5E-3 0.014 |
IEC 60250 |
Condition: Dissipation factor 100 Hz 1.0e+6 Hz |
0.30 0.090 |
IEC 60250 |
Dry: Comparative Tracking Index | 300 V | IEC 60112 |
Condition: Comparative Tracking Index | 300 V | IEC 60112 |